1 ANNEX, Regulation (EU) 2026/331

In forcesince 21 Apr 2026

For the purposes of this Annex, the following symbols apply:

For all classes

ΔΤ | temperature rise

Δm | mass loss

tf | duration of flaming

PCS | gross calorific potential

LFS | lateral flame spread

SMOGRA | smoke growth rate

For all classes except for classes related to electric cables

FIGRA | fire growth rate

THR | total heat release

TSP | total smoke production

Fs | flame spread

For classes related to electric cables only

HRRsm30, kW | heat release rate averaged by a 30-s sliding average

SPRsm60, m2/s | smoke production rate averaged by a 60-s sliding average

Peak HRR, kW | maximum of HRRsm30 between test start and end of test, excluded contribution from ignition source

Peak SPR, m2/s | maximum of SPRsm60 between test start and end of test

THR1200, MJ | total heat release (HRRsm30) from test start until end of test, excluded contribution from ignition source

TSP1200, m2 | total smoke production (SPRsm60) from test start until end of test

FIGRA, W/s | fire growth rate index defined as the highest value of the quotient between HRRsm30 excluding the contribution of ignition source and time. Threshold values HRRsm30 = 3 kW and THR = 0,4 MJ

FS | flame spread (damaged length)

H | flame spread

For the purposes of this Annex the following definitions apply:

(1)

‘material’ means a single basic substance or uniformly dispersed mixture of substances;

(2)

‘homogeneous product’ means a product consisting of a single material, having uniform density and composition throughout the product;

(3)

‘non-homogeneous product’ means a product that does not satisfy the requirements of a homogeneous product and that is composed of one or more components, substantial and/or non-substantial;

(4)

‘substantial component’ means a material that constitutes a significant part of a non-homogeneous product. A layer with a mass per unit area ≥ 1,0 kg/m2 or a thickness ≥ 1,0 mm is considered to be a substantial component;

(5)

‘non-substantial component’ means a material that does not constitute a significant part of a non-homogeneous product. A layer with a mass per unit area < 1,0 kg/m2 and a thickness < 1,0 mm is considered to be a non- substantial component. Two or more non-substantial layers that are adjacent to each other, where there are no substantial components in between the layers, are considered as one non-substantial component and are classified in accordance with the criteria for a layer that is a non-substantial component;

(6)

‘internal non-substantial component’ means a non-substantial component that is covered on both sides by at least one substantial component;

(7)

‘external non-substantial component’ means a non-substantial component that is not covered on one side by a substantial component.

The relevant definitions, tests and performance criteria are fully described or referenced in the relevant harmonised technical specifications, European assessment documents, European reaction to fire classification standards and European testing standards.

[For homogeneous products and substantial components of non-homogeneous products.] [For any external non-substantial component of non-homogeneous products.] [Alternatively, any external non-substantial component having a PCS ≤ 2,0 MJm-2, provided that the product satisfies the following criteria of Single burning item test: FIGRA ≤ 20 Ws-1; and LFS < edge of specimen; and THR600s ≤ 4,0 MJ; and s1; and d0.] [For any internal non-substantial component of non-homogeneous products.] [For the product as a whole.] [s1 = SMOGRA ≤ 30 m2s-2 and TSP600s ≤ 50 m2; s2 = SMOGRA ≤ 180 m2s-2 and TSP600s ≤ 200 m2; s3 = not s1 or s2.] [d0 = no flaming droplets/particles in Single burning item test within 600 s; d1 = no flaming droplets/particles persisting longer than 10 s in Single burning item test within 600 s; d2 = not d0 or d1; Ignition of the paper in Ignitability test results in a d2 classification.] [Under conditions of surface flame attack and, if appropriate to the intended use of the product, edge flame attack.] [No ignition of the paper = no additional classification; Ignition of the paper = d2 classification.]

Class | Test method(s) | Classification criteria | Additional classification

A1 |

Non-combustibility test;

and

ΔΤ ≤ 30 °C;

and

Δm ≤ 50 %;

and

tf = 0 (that is to say, no sustained flaming).

Heat of combustion test |

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 1,4 MJm-2;

and

PCS ≤ 2,0 MJkg-1.

A2 |

Non-combustibility test;

or

ΔΤ ≤ 50 °C;

and

Δm ≤ 50 %;

and

tf ≤ 20 s.

Heat of combustion test;

and

PCS ≤ 3,0 MJkg-1;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 3,0 MJkg-1.

Single burning item test). |

FIGRA0,2MJ ≤ 120 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 7,5 MJ.

Smoke production;

and

Flaming droplets/particles.

B |

Single burning item test;

and

FIGRA0,2MJ ≤ 120 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 7,5 MJ.

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

C |

Single burning item test;

and

FIGRA0,4MJ ≤ 250 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 15 MJ.

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

D |

Single burning item test;

and

FIGRA0,4MJ ≤ 750 Ws-1. |

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

E |

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s. | Flaming droplets/particles

F |

Ignitability test:

Exposure = 15 s.

Fs > 150 mm within 20 s. |

[For homogeneous products and substantial components of non-homogeneous products.] [For any external non-substantial component of non-homogeneous products.] [For any internal non-substantial component of non-homogeneous products.] [For the product as a whole.] [Test duration = 30 minutes.] [Critical flux is defined as the radiant flux at which the flame extinguishes or the radiant flux after a test period of 30 minutes, whichever is the lower (i.e. the flux corresponding with the furthest extent of spread of flame).] [s1 = smoke ≤ 750 %.min; s2 = not s1.] [Under conditions of surface flame attack and, if appropriate to the intended use of the product, edge flame attack.]

Class | Test method(s) | Classification criteria | Additional classification

A1FL |

Non-combustibility test;

and

ΔΤ ≤ 30 °C;

and

Δm ≤ 50 %;

and

tf = 0 (that is to say, no sustained flaming).

Heat of combustion test. |

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 1,4 MJm-2;

and

PCS ≤ 2,0 MJkg-1.

A2FL |

Non-combustibility test;

or

ΔΤ ≤ 50 °C;

and

Δm ≤ 50 %;

and

tf ≤ 20 s.

Heat of combustion test;

and

PCS ≤ 3,0 MJkg-1;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 3,0 MJkg-1.

Determination of the burning behaviour using a radiant heat source test. | Critical flux ≥ 8,0 kWm-2. | Smoke production.

BFL |

Determination of the burning behaviour using a radiant heat source test;

and

Critical flux ≥ 8,0 kWm-2. | Smoke production.

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s.

CFL |

Determination of the burning behaviour using a radiant heat source test;

and

Critical flux ≥ 4,5 kWm-2. | Smoke production.

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s.

DFL |

Determination of the burning behaviour using a radiant heat source test;

and

Critical flux ≥ 3,0 kWm-2. | Smoke production.

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s.

EFL |

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s. |

FFL |

Ignitability test:

Exposure = 15 s.

Fs > 150 mm within 20 s. |

[For homogeneous products and substantial components of non-homogeneous products.] [For any external non-substantial component of non-homogeneous products.] [For any internal non-substantial component of non-homogeneous products.] [For the product as a whole.] [s1 = SMOGRA ≤ 105 m2s-2 and TSP600s ≤ 250 m2; s2 = SMOGRA ≤ 580 m2s-2 and TSP600s ≤ 1 600 m2; s3 = not s1 or s2.] [d0 = no flaming droplets/particles in Single burning item test within 600 s; d1 = no flaming droplets/particles persisting longer than 10 s in Single burning item test within 600 s; d2 = not d0 or d1; Ignition of the paper in Ignitability test results in a d2 classification.] [Under conditions of surface flame attack and, if appropriate to the intended use of the product, edge flame attack.] [No ignition of the paper = no additional classification; Ignition of the paper = d2 classification.]

Class | Test method(s) | Classification criteria | Additional classification

A1L |

Non-combustibility test;

and

ΔΤ ≤ 30 °C;

and

Δm ≤ 50 %;

and

tf = 0 (that is to say, no sustained flaming).

Heat of combustion test. |

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 2,0 MJkg-1;

and

PCS ≤ 1,4 MJm-2;

and

PCS ≤ 2,0 MJkg-1.

A2L |

Non-combustibility test;

or

ΔΤ ≤ 50 °C;

and

Δm ≤ 50 %;

and

tf ≤ 20 s.

Heat of combustion test;

and

PCS ≤ 3,0 MJkg-1;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 4,0 MJm-2;

and

PCS ≤ 3,0 MJkg-1.

Single burning item test. |

FIGRA0,2MJ ≤ 270 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 7,5 MJ.

Smoke production;

and

Flaming droplets/particles.

BL |

Single burning item test;

and

FIGRA0,2MJ ≤ 270 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 7,5 MJ.

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

CL |

Single burning item test;

and

FIGRA0,2MJ ≤ 460 Ws-1;

and

LFS < edge of specimen;

and

THR600s ≤ 15 MJ.

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

DL |

Single burning item test;

and

FIGRA0,4MJ ≤ 2 100 Ws-1;

and

THR600s ≤ 100 MJ.

Smoke production;

and

Flaming droplets/particles.

Ignitability test:

Exposure = 30 s.

Fs ≤ 150 mm within 60 s.

EL |

Ignitability test:

Exposure = 15 s.

Fs ≤ 150 mm within 20 s. | Flaming droplets/particles.

FL |

Ignitability test:

Exposure = 15 s.

Fs > 150 mm within 20 s. |

[For the product as a whole, excluding metallic materials, and for any external component (that is to say, sheath) of the product.] [s1 = TSP1200 ≤ 50 m2 and Peak SPR ≤ 0,25 m2/s; s1a = s1 and transmittance in accordance with Smoke production of burning cable test ≥ 80 %; s1b = s1 and transmittance in accordance with Smoke production of burning cable test ≥ 60 % < 80 %; s2 = TSP1200 ≤ 400 m2 and Peak SPR ≤ 1,5 m2/s; s3 = not s1 or s2.] [The smoke class declared for class B1ca cables must originate from the Burning behaviour and smoke production of bunched cable test (30 kW flame source).] [d0 = no flaming droplets/particles within 1200 s; d1 = no flaming droplets/particles persisting longer than 10 s within 1200 s; d2 = not d0 or d1.] [Acidity of gases produced by burning cables test: a1 = conductivity < 2,5 μS/mm and pH > 4,3; a2 = conductivity < 10 μS/mm and pH > 4,3; a3 = not a1 or a2.] [The smoke class declared for class B2ca, Cca, Dca cables must originate from the Burning behaviour and smoke production of bunched cable test (20,5 kW flame source).]

Class | Test method(s) | Classification criteria | Additional classification

Aca | Heat of combustion test. | PCS ≤ 2,0 MJkg-1. |

B1ca |

Burning behaviour and smoke production of bunched cable test (30 kW flame source);

and

FS ≤ 1,75 m;

and

THR1200s ≤ 10 MJ

and

Peak HRR ≤ 20 kW

and

FIGRA ≤ 120 Ws-1.

Smoke production;

and

Flaming droplets/particles;

and

Acidity (pH and conductivity).

Vertical flame spread of single cable test. | H ≤ 425 mm.

B2ca |

Burning behaviour and smoke production of bunched cable test (20,5 kW flame source);

and

FS ≤ 1,5 m;

and

THR1200s ≤ 15 MJ

and

Peak HRR ≤ 30 kW

and

FIGRA ≤ 150 Ws-1.

Smoke production;

and

Flaming droplets/particles;

and

Acidity (pH and conductivity).

Vertical flame spread of single cable test. | H ≤ 425 mm.

Cca |

Burning behaviour and smoke production of bunched cable test (20,5 kW flame source);

and

FS ≤ 2,0 m;

and

THR1200s ≤ 30 MJ;

and

Peak HRR ≤ 60 kW;

and

FIGRA ≤ 300 Ws-1.

Smoke production;

and

Flaming droplets/particles;

and

Acidity (pH and conductivity).

Vertical flame spread of single cable test. | H ≤ 425 mm.

Dca |

Burning behaviour and smoke production of bunched cable test (20,5 kW flame source);

and

THR1200s ≤ 70 MJ;

and

Peak HRR ≤ 400 kW;

and

FIGRA ≤ 1300 Ws-1.

Smoke production;

and

Flaming droplets/particles;

and

Acidity (pH and conductivity).

Vertical flame spread of single cable test. | H ≤ 425 mm.

Eca | Vertical flame spread of single cable test. | H ≤ 425 mm. |

Fca | Vertical flame spread of single cable test. | H > 425 mm. |

Changed on 21 Apr 2026

TSP1200, m2 | total smoke production (HRRsm60SPRsm60) from test start until end of test